XAR400耐磨钢板焊接指导
发表时间:2018-05-26   浏览次数:2042次

XAR® 400 耐磨钢板焊接指导

 

If due consideration is given to the general rules for welding, this steel is weldable both manually and automatically. To prevent cold cracking in the welded joints only welding consumables giving welds of very low hydrogen content should be used.

 Preheating is not generally necessary for welding with austenitic filler metals.

 For highly stressed weld seams, welded with ferritic filler metals, preheating should in general be used for thicknesses stated in STAHL-EISEN-Werkstoffblatt 088. The preheat temperature level for welding depends on the plate thickness and the residual stress state of the structure. The working temperature should not go beyond 250 °C (482 °F).

 The wear resistance of components fabricated of XAR ® 400 may be increased with the aid of wear resistant layers deposited by means of welding or metal spraying.

 

如果考虑到焊接的一般的要求,手工焊接和自动焊接都适合这种材料是。为了避免在对接焊接处发生冷裂发

生,很重要的一条要注意就是焊材选用含氢量很低的焊材。

 对已奥氏体焊材,XAR® 400 耐磨钢板预热一般情况下是不需要的。

 对于用铁素体焊材焊接有高应力的焊缝,一般情况下在STAHL-EISEN-Werkstoffblatt 088列出的厚度的钢板

应该要预热。温度取决对于钢板的厚度和结构的残余应力。 预热温度不应该高于250 °C。

 由蒂森克虏伯耐磨钢 XAR400 板制作的构件的耐磨性,有可能由于焊接时或金属喷涂时耐磨层的沉积的帮助而提高。

上海志琪实业有限公司,专业从事特种钢板销售及钢板切割加工业务,致力于向客户提供最优质的一站式服务。


  公司的两大事业部:特钢销售部切割加工部一直致力于向您提供更加优质的产品,多年的专注,成就更专业。

http://www.zqsteel.com.cn/show_product.asp?s_id=22